These are five sample questions from Bryq’s Welder assessment, a job-specific test for hiring welders, fabricators and welding technicians. The full assessment covers five skills: welding knowledge, blueprint reading, measurement taking, welding equipment operation and safety standards. Questions combine technical welding knowledge and tolerance calculations with practical workshop scenarios, each with four options to choose from.
Welding Knowledge
Intermediate
Question
Why are low-hydrogen electrodes such as E7018 preferred for welding thick or high-strength structural steel?
Select your answer
They reduce the risk of hydrogen-induced cracking.
They produce a weld that needs no slag removal.
They remove the need for preheat on thick sections.
They deposit metal faster than other stick electrodes.
WHY IS THIS THE CORRECT ANSWER
The low-hydrogen flux coating limits the hydrogen absorbed into the weld. Hydrogen is the main cause of cold cracking in the heat-affected zone of thick or high-strength steel. The benefit only holds if the rods stay dry, which is why they’re kept in heated rod ovens.
Blueprint Reading
Intermediate
Question
A welding symbol shows a fillet weld triangle below the reference line, with the number 6 to its left. What does this specify?
Select your answer
A 6 mm fillet weld on the arrow side of the joint.
Six separate fillet welds on the arrow side.
A 6 mm fillet weld on the other side of the joint.
A fillet weld 6 mm long on the arrow side.
WHY IS THIS THE CORRECT ANSWER
Weld symbols below the reference line apply to the arrow side of the joint, and those above it apply to the other side. The number to the left of the weld symbol gives the weld size (leg length). Length and pitch would appear to its right.
Measurement Taking
Intermediate
Question
A drawing specifies a bevel angle of 30° ± 2.5° on each plate of a single-V groove weld. What is the maximum included angle of the groove?
Select your answer
65°
60°
32.5°
62.5°
WHY IS THIS THE CORRECT ANSWER
The included angle of a single-V groove is the sum of both bevels. At the upper tolerance each bevel can be 32.5°, so the maximum included angle is 2 × 32.5° = 65°.
Welding Equipment Operation
Intermediate
Question
While MIG welding mild steel, the arc becomes erratic and the wire repeatedly burns back to the contact tip. What should be adjusted first?
Select your answer
Increase the wire feed speed, or lower the voltage, to rebalance the arc.
Increase the shielding gas flow rate.
Switch the polarity to DCEN.
Shorten the electrode stickout.
WHY IS THIS THE CORRECT ANSWER
Burnback happens when the wire melts faster than it is fed, usually because the voltage is too high for the wire feed speed. Rebalancing the two restores a stable arc length. A shorter stickout makes burnback worse, and changing gas flow or polarity doesn’t address the cause.
Safety Standards
Intermediate
Question
You’re asked to weld a bracket onto a steel drum that previously held solvent. The drum looks empty and dry. What should you do?
Select your answer
Stop until the drum is cleaned, purged and tested gas-free under a hot work permit.
Weld with an extinguisher nearby, since an empty, dry drum poses little risk.
Rinse the drum with water, let it dry fully, and weld with a fire watch in place.
Remove the bung to vent any vapors for several minutes before welding.
Next